| c-PHDT/GO (%) | Impact strength (KJ/m2) | Flexural modulus (G Pa) | Flexural strength (M Pa) |
| 0 | 1.63 | 8.61 | 41.55 |
| 0.25 | 2.08 | 9.82 | 50.33 |
| 0.5 | 2.30 | 9.9 | 53.87 |
| 0.75 | 2.31 | 10.16 | 54.40 |
| 1.0 | 2.12 | 10.07 | 51.46 |