Alloy | Filler | Heat input, KJ/cm (max) | Shielding gas | Interpass, max |
2003, 2101, 2304 | 2209 | 5 - 25 | Argon + 3%N2 | 150˚C |
2205 | 2209 | 5 - 25 | Argon + 3%N2 | 150˚C |
2507 | 25Cr-10Ni-4Mo-N | 5 - 25 | Argon + 3%N2 | 150˚C |