Sample | Cathode | Electrolyte | Anode | Temp. (˚C) | Resistance (ohm) |
JC806-126-T1 | Li | PC(BN)/LAGP/PC(Li2O) | Li | 24 60 70 80 | −2000 170 120 72.6 |
JC806-126-T2 | Li | PC(BN)/LAGP/PC(Li2O) | Li | 24 60 70 80 | −2000 184 96.0 70.0 |
JC806-126-S1 | Li | Single layer PC(Li2O) | Li | 24 60 70 80 | −3000 190 145 105 |
JC806-126-S2 | Li | Single layer PC(Li2O) | Li | 24 | −2000 |
Cell 6 | 75/25 LAGP/C | PC(BN)/LAGP/PC(Li2O) | Li | 23 60 80 | 3350 320 84 |