Material | Mobility [cm2/V∙s] | Resistivity [Ω∙cm] | Carrier concentration [cm−3] |
AZO | 20 | 5 × 10−4 | 3 × 1020 |
Cu2O (as-grown) | 10 | 560 | 3 × 1015 |
Cu2O (annealed) | 50 | 200 | 1 × 1015 |