Matrix | Coating | Electrolyte Composition | Process conditions | WCA | SA | Ref |
ITO. | Terthiophene (3 T)/ 3 T-Initiator | Surface-initiated atom transfer radical polymerization (SI-ATRP) | 0 - 1.2 V, a scan rate of 10 mV/s, 20 Cycles | 153˚ ± 2˚ | 0˚ | [94] |
ITO. | Perfluoroalkyl alkyl pyrrole | - | 1.25 V (300 s) | 152.3˚ | No SA | [95] |
Gold | PEDOT derivatives | - | 100 mA/cm2 | 159.4˚ | 3.5˚ | [96] |
Gold | Fluorinated polypyrene | Bu 4NClO4 + anhydrous acetonitrile + pyreneMonomers | −0.7 V to EW(1.4 - 1.9 V), a scan rate of 20 mV/s | 160˚ | 1.0˚ | [97] |