Samples | Elongation Strength of Epoxy-Nanocomposites Samples | |||||
Before Artificial Aging | After Artificial Thermal Aging | After Artificial Salt Weathering | ||||
Average Value % | Change % | Average Value % | Change % | Average Value % | Change % | |
Pure epoxy | 9.37 | 0.00 | 7.63 | −18.56 | 8.89 | −5.12 |
Clay/epoxy nanocomposites | 18.42 | +96.58 | 17.49 | −5.04 | 17.99 | −2.33 |
CaCO3/epoxy nanocomposites | 14.18 | +51.33 | 13.61 | −4.01 | 13.89 | −2.04 |
SiO2/epoxy nanocomposites | 11.61 | +23.90 | 10.23 | −11.88 | 10.76 | −7.32 |