| Synthesis Technique | MS (emu/g) | Mr (emu/g) | HC (emu/g) | Applications | Reference |
| Conventional ceramic technique | 61 | 32 | 2080 | HPMR | [68] |
| 49 | 24 | 1050 | HLMR | [69] | |
| 71 | 37 | 4020 | PM | [70] | |
| Coprecipitation technique | 64 | 31 | 4700 | PM | [71] |
| 69 | 36 | 5440 | PM | [75] | |
| 60 | 15 | 860 | HLMR | [72] | |
| Sol-gel technique | 61 | 37 | 4996 | PM | [73] |
| 59 | 36 | 1920 | HPMR | [74] | |
| 61 | 36 | 5692 | PM | [75] | |
| Molten Salt technique | 59 | - | 4820 | PM | [76] |
| 72 | - | 4650 | PM | [77] | |
| 72 | - | 4300 | PM | [77] | |
| Hydrothermal technique | 40 | - | 2500 | PM, HPMR | [77] |
| 59 | 20 | 1350 | HPMR | [78] | |
| 60 | - | 2300 | PM, HPMR | [78] |