| Aluminum | Brass | Magnesium | Zinc |
Tensile strength, MPa | 323.83 | 378.95 | 234.26 | 282.49 |
Yield strength, MPa (0.2% offset) | 15.85 | 20.67 | 15.85 | - |
Shear strength, MPa | 192.92 | 254.93 | 137.8 | 213.59 |
Fatigue strength, MPa | 137.8 | 172.25 | 96.46 | 48.23 |
Elongation % (0.05 m samples) | 3.50 | 15 | 3.0 | 10 |
Hardness (Brinell) | 80 | 91 | 63 | 82 |
Specific gravity (SG) | 2.71 | 8.30 | 1.80 | 6.60 |
Weight, kg/m3 | 2712.6 | 8442.4 | 1826.9 | 6643.2 |
Melting point (liquid), ˚C | 1922.4 | 2948.4 | 1931.4 | 1252.8 |
Thermal conductivity, W/m·K | 0.23 | 0.21 | 0.16 | 0.27 |
Impact strength (Charpy), m/kg | 2.02 | 26.89 | 1.34 | 28.91 |