Material | Bulk density (g/cm3) | Humidity (%) | Pellet diameter (mm) | Pellet width (mm) | Melt flow rate (g/10min) | |
AS-Man | Lab Results | |||||
Recycled PP | 0.574 | 0.590 | 0.137 | 5.036 | 2.016 | 33.8 with 500 g weight at 230˚C |
Recycled HDPE | 0.618 | 0.621 | 0.143 | 4.54 | 3.21 | 1.53 with 500 g weight at 230˚C |