Steel No. | Process | Heat treatment condition | Retained Austenite, % | Mechanical properties measurements | ||||
Temp. ˚C | Time, hr | Y.S (MPa) | U.T.S (MPa) | Elong., % | Reduction of area, % | |||
M3 | IF | 400 | 1 | 1 | 1211 | 1225 | 15 | 45.5 |
ESR1 | 425 | 2 | 7.1 | 1224 | 1239 | 13.7 | 63.3 | |
ESR2 | 425 | 2 | 7.6 | 1327 | 1334 | 14.1 | 53 | |
ESR3 | 425 | 4 | 1.9 | 1114 | 1149 | 11.7 | 45.5 |