| Tensile strength (MPa) | Elastic modulus (GPa) | Elongation (%) | Density (g/cm3) |
Glass | 2300 - 2400 | 70 - 76 | 3 - 3.2 | 2.55 - 2.62 |
Carbon | 4900 | 230 | 2.1 | 1.8 |
Vinyl Ester | 69-89 | 3 | 6.0 - 8.0 | 1.2(25˚C) |