Material | Trial conditions | |||
Liquid nitrogen, −195˚C | Dr y nitrogen 240˚C | Water-saturated steam | ||
240˚C | 25˚C | |||
Quartz glass (compression) | 4600 | 4530 | 2570 | 3910 |
Granite (compression) | 2620 | 1380 | 420 | 1640 |
Spodumen (Compression) | 6680 | 4020 | 3200 | 2710 |
Quartz (compression) | 5720 | 4480 | 2510 | 3670 |
MgO-Crystal (bending) | 2140 | 1870 | 560 | 1000 |
Al2O3 Crystal (bending) | 10,700 | 8200 | 4800 | 7730 |