Samples | Lattice Spacings and Relative Intensities | Crystal Phase | |||
Standard SS-304 [PDF no. 33 - 397] | |||||
d (Å) | 2.08 | 1.80 | 1.27 | - | Austenitic Steel |
I/Io | 100.0 | 50.0 | 30.0 | - | Cr0.19Fe0.70Ni0.11 |
SSPN: | |||||
d (Å) | 2.0803 | 1.8041 | 1.2746 | - | Austenite+ |
I/Io | 100.0 | 67.6 | 87.1 | - | Unknown phase |
SSDN: | |||||
d (Å) | 2.0708 | - | 1.2706 | - | Austenite+ |
I/Io | 100.0 | - | 67.7 | - | Unknown phase |
SSOP: | |||||
d (Å) | 2.0735 | 1.7940 | 1.2694 | 3.0502 | Austenite+ |
I/Io | 100.0 | 47.1 | 25.8 | 65.0 | Unknown phase |