Author

Wood species

Treatment method

Product

Dimension of samples mm

Volume mm3

Retention (Kg/m3)

(Ozdemir, T., et al., 2015) [7]

Pinus sylvestris L.

Vacuum (45 m)

Tanalith E (2%)

300 × 100 × 15

450,000

15.39

(Ozdemir, T., et al., 2015) [7]

Pinus sylvestris L.

Vacuum (45 m)

CCA (2%)

300 × 100 × 15

450,000

15.67

(Ozdemir, T., et al., 2015) [7]

Pinus sylvestris L.

Vacuum (45 m)

Boric acid (1%)

300 × 100 × 15

450,000

6.92

(Chong, S., 1977) [8]

Pinus radiata D.

Vacuum and pressure

CCA (2%)

4.3 × 50 × 25

5375

13.3

(Yildiz, U. et al., 2004) [9]

Pinus sylvestris L.

Vacuum (60 m)

CCA (2%)

5 × 10 × 100

5000

13.24

(Yildiz, U. et al., 2004) [9]

Pinus sylvestris L.

Vacuum (60 m)

Tanalith E 3491 (2%)

5 × 10 × 100

5000

11.64

(Yildiz, U. et al., 2004) [9]

Pinus sylvestris L

Vacuum (60 m)

ACQ-1900 (2%)

5 × 10 × 100

5000

12.99

(Yildiz, U. et al., 2004) [9]

Pinus sylvestris L

Vacuum (60 m)

Wolmanit CX-8 (2%)

5 × 10 × 100

5000

13.04

(Yildiz, S., 2007) [10]

Pinus sylvestris L. ssp.

Vacuum and pressure

Tanalith E 3492 (2.4%)

50 × 50 × 100

762,000

4.95

(Yildiz, S., 2007) [10]

Pinus sylvestris L. ssp.

Vacuum and pressure

Tanalith E 3492 (2.4%)

50 × 100 × 152.4

762,000

2.48