B (Gpa) | G (Gpa) | E (Gpa) | CSS (GPa) | Toughness (J/m3) × 106 | Fracture Strength (MPa) | Yield strength (MPa) | Tensile strength (MPa) | Alloy |
49.2 | 16.1 | 43.6 | 9.2 | 2.83 | 167.2 | 178.3 | 154.6 | Al-0.1%Zn-0.2%Sn-0.22%Bi |
129.4 | 39.6 | 107.2 | 9.7 | 15.80 | 431.6 | 393.9 | 431.5 | Al-0.1%Zn-0.5%Sn-0.54%Bi |
134.6 | 43.0 | 116.6 | 15 | 2.98 | 315.6 | 274.3 | 315.5 | Al-0.1%Zn-1%Sn-1.08%Bi |
75.5 | 24.8 | 67.1 | 9.3 | 4.39 | 283.7 | 255.4 | 284.4 | Al-0.1%Zn-1.5%Sn-1.63%Bi |