| Condition | Quantity |
| Copper | 13 g/L |
| Temperature | 30˚C - 35˚C |
| Anode current density | Low—400 A/m2; High—550 A/m2 |
| Cathode current density | Low—800 A/m2; High—1100 A/m2 |
| Cell potential | 5 V |
| Additives | 1 wt% boric acid or glycerine |