| Bridge Name | Girder No. | Deterioration Condition* | Suitable Method of Rehabilitation |
| Al-Qadisia Bridge | 1 | Severe damage on the eastern side | Immediate replacement of the deficient part |
| 2 | Severe damage on the eastern side | Immediate replacement of the deficient part | |
| 3 | Minor damage on the eastern side | Cleaning out the loose concrete and apply epoxy to the rebar. [10] [11] | |
| 4 | Moderate damage on the eastern side | Immediate rehabilitation by preparing the surface and applying FRP composites. [10] [11] [12] . | |
| 5 | Moderate damage on the eastern side | Immediate rehabilitation by preparing the surface and applying FRP composites. [10] [11] [12] . | |
| 6 | Moderate damage on the western side | Immediate rehabilitation by preparing the surface and applying FRP composites. [10] [11] [12] . | |
| 7 | Moderate damage on the western side | Immediate rehabilitation by preparing the surface and applying FRP composites. [10] [11] [12] . | |
| 8 | Minor damage on the western side | Cleaning out the loose concrete and apply epoxy to the rebar. [10] [11] | |
| 9 | Minor damage on the western side | Cleaning out the loose concrete and apply epoxy to the rebar. [10] [11] | |
| 10 | Severe damage on the western side | Immediate replacement of the deficient part | |
| Unayza-Petra Bridge | 1 | Severe damage on the western side | Immediate replacement of the deficient part |
| 2 | Moderate damage on the western side | Immediate rehabilitation by preparing the surface and applying FRP composites. [10] [11] [12] . | |
| 3 | Moderate damage on the western side | Immediate rehabilitation by preparing the surface and applying FRP composites. [10] [11] [12] . | |
| 4 | Minor damage on the western side | Cleaning out the loose concrete and apply epoxy to the rebar. [10] [11] | |
| 5 | Minor damage on the eastern side | Cleaning out the loose concrete and apply epoxy to the rebar. [10] [11] | |
| 6 | Minor damage on the eastern side | Cleaning out the loose concrete and apply epoxy to the rebar. [10] [11] | |
| 7 | Moderate damage on the eastern side | Immediate rehabilitation by preparing the surface and applying FRP composites. [10] [11] [12] . |