δ | TC (K) | c (Å) | a (Å) | Cooling condition | Sample |
0.189 | 110
| 33.78 | 4.350 | Furnace cooled | Tl2Sr2Ca2Cu3O10+δ |
0.250 | 118 | 34.37 | 4.150 | Quenched in air | |
0.298 | 120 | 37.616 | 3.721 | Furnace cooled | Tl1.6Hg0.4Sr2Ca2Cu3O10+δ |
0.301 | 130 | 37.889 | 4.056 | Quenched in air |