Entry | Catalyst | Methods | Conversion (%) | Selectivity (%) | Reference |
1 | Zr(CO3)x | aqueous solution | 100 | C9:92 | 13 |
2 | MgO-ZrO2 | aqueous solution | 93.3 | aldol product: 55.9 C9:50.4, C15:49.6 | 25 |
3 | MgAl | aqueous solution | 27.2 | C9:25.6, C15:17.1 | 14 |
4 | MgZr | aqueous solution | 53.4 | C9:43.4, C15:49.6 | 14 |
5 | CO2 | 200˚C, CO2 MPa | >95% | C9 > 95% | 26 |
6 | Cu/MgAl2O4 | Acetone as solvent | 100 | C9:78, C15:7 | 27 |
7 | FAU-type zeolite nanosheets | Solvent free | 91.74 | C9: close to 100% | 28 |