Name | Particle diameter (mm) | Surface area (m2/g) | Average pore diameter (nm) | Polarity |
NKA-9 | 0.3 - 1.25 | 250 - 290 | 15.5 - 16.5 | Polar |
NKA | 0.3 - 1.25 | 160 - 200 | 14.5 - 15.5 | Polar |
D101 | 0.3 - 1.25 | ³400 | 9.0 - 11.0 | Non-polar |
AB-8 | 0.3 - 1.25 | 480 - 520 | 13.0 - 14.0 | Weak-polar |
HPD-750 | 0.3 - 1.25 | 650 - 700 | 8.5 - 9.0 | Mild-polar |