Polyester satin 4 weave

Weft count (18/2S)

Weft count (24/2S)

Weft count (40/2S)

Pulsing rate (P/min)

Pulsing rate (P/min)

Pulsing rate (P/min)

3

6

9

3

6

9

3

6

9

% Change Sample weight after pulsing (gm)

+7.0

+6.7

+5.8

+9.6

+8.0

+6.7

+9.7

+9.3

+9.3

% Change in Rate of Air-permeability after pulsing

−39

−38

−34

−36.5

−34.0

−30.7

−47

−39

−32.5

Sample thickness

(mm)

+3.6

+1.8

+0.0

+1.8

+0.93

+0.0

+0.0

0.0

+1.0

Fabric dust holding capacity (%)

+2.0

+1.9

+1.7

+2.6

+2.1

+1.8

+2.1

+2.1

+2.2

Polyester basket weave

Weft count (18/2S)

Weft count (24/2S)

Weft count (40/2S)

Pulsing rate (P/min)

Pulsing rate (P/min)

Pulsing rate (P/min)

3

6

9

3

6

9

3

6

9

% Change Sample weight after pulsing (gm)

+8.5

+6.8

+4.9

+5.6

+5.0

+4.7

+11.6

+10.0

+9.3

% Change in Rate of Air-permeability after pulsing

−37.7

−30.2

−29.3

−39.7

−36.9

−35.6

−49

−47

−43.4

Sample thickness

(mm)

0.0

0.0

0.0

0.0

0.0

0.0

0.0

0.0

0.0

Fabric dust holding capacity (%)

+2.4

+1.9

+1.4

+1.9

+1.6

+1.5

+2.6

+2.3

2.1