| FP parameters | Description |
| Ld = 400 μm | Cavity length |
| d = 0.2 μm | Active region thickness |
| w = 2 μm | Active region width |
| No = 1 × 1024 m−3 | Transparency carrier density |
| dNo/dT = 4 × 1021 m−3∙K−1 | Transparency carrier density temperature dependence |
| Anr = 1 × 108 sec−1 | Nonradiative recombination coefficient |
| B = 1 × 10−16 m3/sec | Radiative recombination coefficient |
| C = 3 × 10−41 m6/sec | Auger recombination coefficient |
| dC/dT = 0.027 × 10−41 m6∙s−1∙K−1 | Auger recombination coefficient temperature dependence |
| αint = 1000 m−1 | Internal cavity loss |
| dαint/dT = 3.33 × 10−3 cm−1∙K−1 | Internal cavity loss temperature dependence |
| Γ = 0.34 | Field confinement factor |
| R1 = 0.9 | High reflectivity (HR) of the left facet |
| nd = 4 | Group refractive index |
| dnd/dT = 2.5 × 10−4 K−1 | Active region refractive index temperature dependence |
| ao = 2.5 × 10−20 m2 | Differential gain |
| dao/dT = −2 × 10− 23 m2 ∙K−1 | Gain coefficient temperature dependence |
| α = 5 | Linewidth enhancement coefficient |
| βsp = 1 × 10−5 | spontaneous-emission factor |
| Iinj = 4 Ith | Injection current |
| next = 1.44 | Fiber refractive index |
| dnext/dT = 1.6 × 10−5 K−1 | Fiber refractive index temperature dependence |
| LFG = 4 mm | Grating length |