Treatments (Levels of Substitution, %)

Average Flexural Strength (MPa)** of Concrete Tiles

With Pulverized Aluminized Plastic Wrappers

With Pulverized Clear Plastic Wrappers

0 (LS1)

0.893a

0.893a

15 (LS2)

0.398b

0.505b

30 (LS3)

0.378bc

0.414bc

45 (LS4)

0.367bc

0.243c