Diode laser beam spot (FWHM) | 17 mm × 2 mm |
Shroud gas | Argon at 3 bar |
Scanning speed (for power ramping experiments) | 6 mm/s |
Laser power (for power ramping experiments) | 500 - 1700 W |
Temperature range (for power ramping experiments) | 800˚C - 1320˚C |
Laser power (for texturing experiments) | 6000 W |
Interaction time (for texturing experiments) | 3.3 - 100 ms |
Sample condition | Surface ground to 1.2 µm Ra finish |