| Densities (g/cm3) | Actual pulp fibre content |
Polyamide 11 (PA11) reinforced HYP fibre composite: Extrusion compounding technique | ||
PA11 | 1.03 | 0 |
PA11 + 10% HYP | 1.05 | 12.5% |
PA11 + 20% HYP | 1.07 | 25% |
PA11 + 30% HYP | 1.12 | 33.2% |
Modified Polyamide 11 (PA11) reinforced HYP fibre composite: Brabender mixer technique | ||
PA11 + 3%LiCl + 10% HYP | 1.07 | 14% |
PA11 + 3%LiCl + 20% HYP | 1.11 | 26% |
PA11 + 3%LiCl + 30% HYP | 1.21 | 38.3% |