| Lifetime (sec) | |||
|
| ILGAR | Spin coating | ||
| Laser intensity | As deposited | Annealed | As deposited | Annealed |
| 35 μJ | 2.85 × 10−5 | 3.18 × 10−5 | 1.36 × 10−5 | 0.78 × 10−5 |
| 14 μJ | 2.22 × 10−5 | 2.26 × 10−5 | 1.36 × 10−5 | 0.75 × 10−5 |
| 7 μJ | 1.51 × 10−5 |
| 1.36 × 10−5 |
|
| 3.5 μJ | 1.56 × 10−5 | 1.45 × 10−5 | 1.36 × 10−5 | 0.7 × 10−5 |
| 1.4 μJ | 1.3 × 10−5 |
| 1.34 × 10−5 |
|