Samples | Compressive Strength of Epoxy-Nanocomposites Samples | |||||
Before Artificial Aging | After Artificial Thermal Aging | After Artificial Salt Weathering | ||||
Average Value (kg/cm2) | Change % | Average Value (kg/cm2) | Change % | Average Value (kg/cm2) | Change % | |
Pure epoxy | 125.53 | 0.00 | 120.60 | −3.92 | 124.11 | −1.13 |
Clay/epoxy nanocomposites | 133.89 | +6.65 | 131.22 | −1.99 | 133.11 | −0.58 |
CaCO3/epoxy nanocomposites | 129.84 | +3.43 | 126.84 | −2.31 | 128.98 | −0.66 |
SiO2/epoxy nanocomposites | 127.80 | +1.80 | 123.40 | −3.44 | 126.88 | −0.71 |