Process | Percent of glass fiber by weight | Tensile strength (ksi) | Tensile modulus (103 ksi) | Flexural Modulus (ksi) | Compressive strength (ksi) |
Filament winding (glass-polymer) | 40 - 75 | 35 - 50 | 2500 - 3600 | 30 - 50 | 30 - 45 |
Pultrusion (glass-matt polymer) | 40 - 80 | 60 - 150 | 4000 - 6000 | 100 - 150 | 30 - 70 |
Pultrusion (glass mat and roving polymer) | 30 - 55 | 7 - 35 | 800 - 2500 | 10 - 30 | 15 - 40 |
Centrifugal casting | 40 - 45 | 30 - 40 | 2200 - 2500 | 30 - 40 | 25 - 35 |
Hand lay up | 40 - 75 | 30 - 40 | 800 - 2500 | 10 - 30 | 15 - 40 |