| Oxides | ADR fines directly used in C2CA trial | FF (0 - 0.125 mm) resulted from heating and grinding | Example Clay | 65% CaCO3 (marl) Limestone-low quality | 95% CaCO3 Limestone-high quality |
| SiO2 | 75.49 | 41.2 | 67.30 | 21.80 | 2.83 |
| Al2O3 | 4.57 | 6.42 | 9.00 | 5.48 | 0.69 |
| TiO2 | 0.23 | 0.41 | - | 0.26 | 0.03 |
| MnO | 0.13 | 0.13 | - | 0.03 | 0.03 |
| Fe2O3 | 1.64 | 2.97 | 4.30 | 1.86 | 0.28 |
| CaO | 11.24 | 35.16 | 7.30 | 36.60 | 53.00 |
| MgO | 1.23 | 1.79 | 2.00 | 0.87 | 0.61 |
| K2O | 0.85 | 0.78 | 1.20 | 0.97 | 0.13 |
| Na2O | 0.43 | - | 1.40 | 0.13 | 0.04 |
| SO3 | 0.78 | 1.75 | 0.30 | 0.56 | 0.04 |
| P2O5 | 0.07 | - | - | 0.08 | 0.06 |
| LOI | 9.03 | 9.13 | 7.20 | 30.88 | 41.90 |