Samples | Storage modulus (Pa) | Tan delta | Tg* (˚C) | Modulus at Tg | Tan delta at Tg | ||||
30˚C | 70˚C | 140˚C | 30˚C | 70˚C | 140˚C | ||||
PVC/2 phr com. therm. stab. | 1.70E09 | 1.67E08 | 3.25E06 | 0.024 | 0.074 | 0.142 | 76.2 | 3.68E7 | 1.005 |
PVC/1 phr tannin-Ca complex | 1.716E09 | 1.97E08 | 3.00E06 | 0.033 | 0.737 | 0.173 | 75.9 | 3.95E07 | 1.115 |
PVC/2 phr tannin-Ca complex | 1.88E09 | 2.60E08 | 3.324E6 | 0.0236 | 0.653 | 0.154 | 76.8 | 4.04E07 | 1.113 |
PVC/3 phr tannin-Ca complex | 1.90E9 | 2.06E08 | 2.88E6 | 0.0223 | 0.731 | 0.127 | 76.1 | 4.312E07 | 1.112 |